Durability engineering
Concrete durability engineering and service-life design
Each asset is designed for how it will perform at 10, 25, 50 and 100 years, from the first exposure assessment through modelling, durability reports and a durability management plan to the as-built record.
Interactive model
Cover and mix selected for the design life, not read from a table
Explore how binder type, cover, exposure and temperature change the time to corrosion initiation.
Illustrative deterministic calculation in the fib Bulletin 34 format (C0 = 0, kt = 1, t0 = 28 days, be = 4800 K). Starting values are examples only; a project assessment uses measured NT Build 492 results, site exposure data and semi-probabilistic or full-probabilistic analysis. Not for design.
Deemed-to-satisfy
AS 3600 and AS 5100.5 Section 4 tables for cover, grade and curing. Design life of about 50 years in standard exposure.
Deterministic
Mean-value chloride and carbonation models for concept options, mix comparison and cover optimisation.
Semi-probabilistic
Partial factor format of fib Bulletin 34 for 100-year assets designed to an owner's durability specification.
Full-probabilistic
Monte Carlo simulation reporting the probability of depassivation and the reliability index at 10, 25, 50 and 100 years.
Exposure, mechanism and control
Every durability report starts from the exposure
Each element is classified, its governing deterioration mechanism identified, and controls chosen that can be verified on site.
Marine tidal, splash and spray
Chloride-induced corrosion and salt crystallisation. Blended binders, low water to binder ratio, increased cover, crack-width limits and probabilistic chloride modelling.
Coastal atmospheric
Chloride ingress and carbonation. Cover and grade to AS 3600 Tables 4.10.3.2 and 4.10.3.3, curing to Table 4.4, steelwork coatings to the AS 4312 category.
Water-retaining and wastewater
Leaching, chloride and sulfate attack, and microbially induced corrosion. Crack-width limits for tightness and early-age thermal control.
Aggressive soils and groundwater
Sulfate and acid attack, including acid sulfate soils. Exposure class from soil chemistry, Type SR cement, increased cover and membranes.
Internal and dry
Carbonation-induced corrosion. Deemed-to-satisfy cover and grade, with a carbonation check for long design lives.
Industrial and thermal
Chemical attack, thermal cycling and abrasion. Binder performance specification, surface protection and inspection intervals matched to the process.
Durability deliverables at every project stage
| Stage | Deliverable | Content |
|---|---|---|
| Concept and tender | Durability philosophy and preliminary assessment | Design-life strategy, exposure zoning, governing mechanisms, and cost-relevant options such as binder type, cover, coatings and stainless reinforcement |
| Detailed design | Durability design report | Element-by-element exposure classes, modelling results, concrete, cover and crack-width requirements, steel protection and specification inputs |
| Issued for construction | Durability requirements register and specification clauses | Measurable requirements with acceptance tests and hold points, aligned to the drawings and the project specification |
| Construction | Durability management plan and compliance reviews | Mix approvals, prequalification testing, cover and curing controls, and durability assessment of non-conformances |
| Handover | As-built durability report | Achieved cover and test results, updated service-life prediction from as-built data, and the inspection and maintenance plan |
| Operation | Durability assessment of existing structures | Condition survey interpretation, residual service life and repair and protection strategy |
Durability management plans
A durability management plan carries the durability design through construction and into operation, assigning each requirement an owner, a verification method and a record: requirements register, roles and responsibilities, materials approval, construction controls with hold points for spacers and cover, non-conformance management, the as-built durability record, operation and maintenance, and a review cycle after each principal inspection.
Standards and guidance
AS 3600 Section 4; AS 5100.5 Section 4; AS 3735 and Supplement 1; AS 4997; AS 2159; AS 1379; AS 3972; AS 3582 series; AS 1012 series; NT Build 492 and NT Build 443; fib Model Code 2010; fib Bulletin 34; ISO 16204; ISO 13823; AS 4312; AS/NZS 2312.1 and 2312.2; AS/NZS 4680; AS 2832.5; EN 1504; Concrete Institute of Australia Z7 series; CIRIA C660; Main Roads WA and Water Corporation concrete and durability specifications.
Questions
What design life do the AS 3600 durability tables cover?
AS 3600 Section 4 provides deemed-to-satisfy durability provisions for a design life of 50 years plus or minus 20 per cent (cl. 4.1).
Which models are used for chloride ingress and carbonation?
Chloride ingress uses the error-function solution of Fick's second law in the fib Bulletin 34 and fib Model Code 2010 format, with a time-dependent apparent diffusion coefficient. Carbonation uses the fib Bulletin 34 carbonation model. Both are evaluated against the depassivation limit state.
How are model inputs checked during construction?
Inputs are tied to measurable acceptance tests, such as chloride migration to NT Build 492 and volume of permeable voids to AS 1012.21, so the design assumption can be verified on site.
Can you assess an existing structure?
Yes. Condition surveys are planned and cover meter, carbonation depth, chloride profile, half-cell potential (ASTM C876) and core results (AS 1012.14) are interpreted to recalibrate the models, estimate residual service life and set a repair strategy consistent with EN 1504.
Need a durability report or management plan?
Talk directly to the engineer who will do the work.